Abstract:Density functional simulations have been performed for Pt n Ni 55−n clusters (n = 0,12,20,28,42,55) to investigate their catalytic properties for the hydrogen evolution reaction (HER). Starting from the icosahedral Pt 12 Ni 43 , hydrogen adsorption energetics and electronic d-band descriptors indicate HER activity comparable to that of pure Pt 55 (distorted reduced core structure). The PtNi clusters accommodate a large number of adsorbed hydrogen before reaching a saturated coverage, corresponding to 3–4 H atoms per icosahedron facet (in total ∼70–80). The differential adsorption free energies are well within the window of |∆GH| < 0.1 eV which is considered optimal for HER. The electronic descriptors show similarities with the platinum d-band, although the uncovered PtNi clusters are magnetic. Increasing hydrogen coverage suppresses magnetism and depletes electron density, resulting in expansion of the PtNi clusters. For a single H atom, the adsorption free energy varies between -0.32 (Pt 12 Ni 43 ) and -0.59 eV (Pt 55 ). The most stable adsorption site is Pt–Pt bridge for Pt-rich compositions and a hollow site surrounded by three Ni for Pt-poor compositions. A hydrogen molecule dissociates spontaneously on the Pt-rich clusters. The above HER activity predictions can be extended to PtNi on carbon support as the interaction with a graphite model structure (w/o vacancy defect) results in minor changes in the cluster properties only. The cluster-surface interaction is the strongest for Pt 55 due to its large facing facet and associated van der Waals forces.
physics, condensed matter
What problem does this paper attempt to address?