Isocyanate Reduction by Epoxide Substitution of Alcohols for Polyurethane Bioelastomer Synthesis

Arnold A. Lubguban,Zuleica R. Lozada,Yuan-Chan Tu,Hongyu Fan,Fu-Hung Hsieh,Galen J. Suppes
DOI: https://doi.org/10.1155/2011/936973
2011-01-01
International Journal of Polymer Science
Abstract:A phosphate ester-forming reaction was carried out by mixing epoxidized soybean oil with up to 1.5% o -phosphoric acid. In situ oligomerization took effect almost instantly producing a clear, homogeneous, highly viscous, and a low-acid product with a high average functionality. The resulting epoxide was used as a reactant for urethane bioelastomer synthesis and evaluated for rigid foam formulation. Results have shown that with a number of catalysts tested phosphoric acid significantly enhances a solvent-free oxirane ring cleavage and polymerization of the epoxidized soybean oil via phosphate-ester formation at room temperature. The resulting phosphoric acid-catalyzed epoxide-based bioelastomer showed an 80% decrease in extractable content and increased tensile strength at the same isocyanate loading relative to the noncatalyzed epoxide. The oligomerized epoxidized soybean oil materials exhibited ASTM hydroxyl values 40% less than the nonoligomerized starting material which translates to reduced isocyanate loadings in urethane applications.
polymer science
What problem does this paper attempt to address?