Leaching of coal fly ash with sulphuric acid for synthesis of wastewater treatment composite coagulant
M. Clotilde Apua,B. Diakanua Nkazi
DOI: https://doi.org/10.1080/00084433.2022.2044689
2022-03-04
Canadian Metallurgical Quarterly
Abstract:The results of leaching of coal fly ash in H2SO4 solution are presented. The effects of leaching time, H2SO4 concentration, temperature, and solid/liquid ratio were explored for the dissolution process. Particle size distribution results showed that changes in particle size occurred during the dissolution process; XRD, XRF and FTIR results indicated the same characteristics of the mineral matter in the raw and treated coal fly ash samples; and SEM showed that the raw coal fly ash particles have smooth spherical surfaces while a pricked and corroded surface and a stem-like structure were formed after leaching. The dissolution rate of coal fly ash is controlled by mixed-controlled mechanism (diffusion and chemical reaction). The corresponding activation energies were calculated to be 59.8 kJ/mol for iron, 7.3 kJ/mol for aluminium and 5.8 kJ/mol for silicon. The reaction order was determined to be zero order kinetic model.
metallurgy & metallurgical engineering
What problem does this paper attempt to address?