Injectable, Non‐Diffusible, and Pre‐Filled Bone Paste Composed of α‐Tricalcium Phosphate and Hydrophobically Modified Poly(Vinyl Alcohol)

Xi Chen,Tetsushi Taguchi
DOI: https://doi.org/10.1002/adem.201900660
IF: 3.6
2019-09-11
Advanced Engineering Materials
Abstract:In this study, injectable, non‐diffusible, and pre‐filled bone pastes were developed using α‐tricalcium phosphate (α‐TCP) and hydrophobically modified poly(vinyl alcohol)s (hm‐PVAs) with various alkyl chain lengths (3–12). The resulting bone pastes showed high injectability (over 90%) when the solid‐liquid ratio was lower than 3.5. The non‐diffusion property of α‐TCP/hm‐PVAs bone pastes in water and fresh porcine blood was observed compared with α‐TCP alone, α‐TCP/original PVA (Org‐PVA), and commercial calcium phosphate paste. Compressive strength of α‐TCP/nonanal modified PVA (C9‐PVA) bone pastes was 5.4 ± 1.4 MPa within 24 h, and reached to 27.5 ± 2.7 MPa after 7 days in water. Young's modulus of α‐TCP/C9‐PVA bone pastes was 0.84 ± 0.02 GPa, which was lower than that of commercial calcium phosphate paste (1.5 ± 0.02 GPa) and poly(methyl methacrylate)‐based bone cement (1.06 ± 0.03 GPa). Furthermore, the surface of α‐TCP/C9‐PVA bone pastes showed excellent cell adhesion of cultured osteoblastic cells. These results demonstrated that α‐TCP/C9‐PVA bone paste is a promising bone filler for percutaneous vertebroplasty (PVP) surgery.This article is protected by copyright. All rights reserved.
materials science, multidisciplinary
What problem does this paper attempt to address?