Initial investigation into the leaching of manganese from nodules at room temperature with the use of sulfuric acid and the addition of foundry slag—Part II

Kevin Pérez,Ángelo Villegas,Manuel Saldaña,Ricardo I. Jeldres,Javier González,Norman Toro
DOI: https://doi.org/10.1080/01496395.2020.1713816
IF: 2.799
2020-01-09
Separation Science and Technology
Abstract:The marine nodules are an attractive alternative source for the extraction of manganese due to the scarcity of high-grade metals on the surface. In the present investigation, working parameters (Fe<sub>2</sub>O<sub>3</sub>/MnO<sub>2</sub> ratio and sulfuric acid concentration) were optimized for the dissolution of Mn from marine nodules using foundry slags. Finally, it is concluded that the optimum MnO<sub>2</sub>/Fe<sub>2</sub>O<sub>3</sub> proportion is 1/2, while the optimum concentration of H<sub>2</sub>SO<sub>4</sub> is 0.3 mol/L for a leaching time of 20 minutes achieving solutions of 70% Mn.
engineering, chemical,chemistry, multidisciplinary
What problem does this paper attempt to address?