Rational Design of Sandwich-Like “Gel–Liquid–Gel” Electrolytes for Dendrite-Free Lithium Metal Batteries

Fan Yang,Wang Sun,Yu Bai,Tianye Xu,Kedi Cai,Huiqun Cai,Kening Sun,Zhenhua Wang
DOI: https://doi.org/10.1021/acs.iecr.0c00254
2020-07-20
Abstract:Issues of lithium dendrite growth still hinder the popular application of lithium metal batteries (LMBs). Herein, we demonstrate that "gel–liquid–gel" electrolytes effectively suppress the growth of dendrites. This sandwich structure is based on introducing gel polymer coating layers, which consist of polyvinylidene fluoride-hexafluoropropylene (PVDF-HFP), onto both sides of a Celgard separator. The PVDF-HFP layers improve the overall liquid electrolyte retention and compatibility with lithium anodes. They also lead to a uniform Li-ion flux at the polymer/lithium interface, which results in the suppression of dendrite nucleation. Impressively, Li|Cu cells operate stably for over 400 cycles with a high Coulombic efficiency of ∼98%. Li|Li symmetric cells enable highly stable Li plating/stripping cycling for over 1200 h at 1 mA cm<sup>–2</sup>. Li|LiFePO<sub>4</sub> full cells also exhibit excellent cycling performance. We expect this work to have great potential in the application of simple composite gel polymer electrolytes to achieve highly safe LMBs.The Supporting Information is available free of charge at <a class="ext-link" href="/doi/10.1021/acs.iecr.0c00254?goto=supporting-info">https://pubs.acs.org/doi/10.1021/acs.iecr.0c00254</a>.Illustration of semisolid-state battery design with the GLGE; cross-sectional SEM image of the pure PVDF-HFP membrane; impedance spectra of the Celgard separator, composite separator, and PVDF-HFP membrane in SS|SS cells; current–time plots of Celgard and the GLGE symmetric Li cell with a liquid electrolyte of 1.0 M LiPF<sub>6</sub> in a 1:1 (by volume) mixture of DEC and EC after the application of a constant potential (20 mV) and the inserts are the impedance spectra before (solid circle) and after (hollow circle) polarization; cycling stability of the pristine GLGE at a current density of 1 mA cm<sup>–2</sup> with the areal capacity limit of 1 mA h cm<sup>–2</sup> in a Li|Li cell; and cycling performance of the battery with the GLGE at a rate of 2 C (<a class="ext-link" href="/doi/suppl/10.1021/acs.iecr.0c00254/suppl_file/ie0c00254_si_001.pdf">PDF</a>)This article has not yet been cited by other publications.
engineering, chemical
What problem does this paper attempt to address?