Hydrogen embrittlement resistance of pre-strained ultra-high-strength low alloy TRIP-aided steel

Tomohiko Hojo,Bakuya Kumai,Motomichi Koyama,Eiji Akiyama,Hiroyuki Waki,Hiroyuki Saitoh,Ayumi Shiro,Ryo Yasuda,Takahisa Shobu,Akihiko Nagasaka
DOI: https://doi.org/10.1007/s10704-020-00451-5
IF: 2.635
2020-06-08
International Journal of Fracture
Abstract:In the study, the pre-strain effect on hydrogen embrittlement property of the ultra-high-strength transformation-induced plasticity (TRIP)-aided bainitic ferrite (TBF) steel was investigated towards application for automobile frame parts. Specifically, 3–10% tensile pre-strain suppressed hydrogen-induced mechanical degradation relative to total elongation (pre-strain <span class="mathjax-tex">\(+\)</span> elongation after hydrogen charging) while 12–15% pre-strained specimen did not exhibit elongation after hydrogen charging. The advantageous effect of the 3–10% pre-strain was attributed to the suppression of crack initiation related to retained austenite. Specifically, the TRIP by pre-straining decreased the volume fraction of retained austenite before hydrogen charging, thereby reducing existing probabilities of preferential crack initiation sites and propagation paths. Conversely, high pre-strain such as 12–15% does not effectively work due to work hardening resulting in increases in hydrogen embrittlement susceptibility and a significant increase in hydrogen content due to the multiplication of dislocations.
mechanics,materials science, multidisciplinary
What problem does this paper attempt to address?