Anisotropic Carbon Aerogel from Cellulose Nanofibers Featuring Highly Effective Compression Stress Transfer and Pressure Sensing

Haihong Lai,Hao Zhuo,Yijie Hu,Ge Shi,Zehong Chen,Linxin Zhong,Meiyun Zhang
DOI: https://doi.org/10.1021/acssuschemeng.1c02051
2021-07-13
Abstract:Carbon aerogels with excellent compressibility and resilience are attracting considerable attention in broad application prospects for their reversible resilience and resistance to damage from external stress. It is of great interest to explore green and low-cost carbon aerogels from sustainable resources but remains challenging because of the brittleness of carbon blocks. Herein, inspired by the anisotropic architectures in nature, we propose a bottom-up approach for fabricating an anisotropic carbon aerogel with a 3D lamellar structure from cellulose nanofibers. The aligned and continuous lamellar texture with desirable thickness (142 nm) can effectively transfer stress throughout the 3D network and resist the destruction at high compression, and thus, the carbon aerogel exhibits shape recovery from high compression strain and excellent fatigue resistance. The carbon aerogel can withstand extremely high compression strain (95%) for at least 50 cycles or 50,000 cycles at 50% strain with 84% height retention. Moreover, the excellent mechanical performance, stable 3D lamellar architecture, and high conductivity endow the carbon aerogel with rapid current response and high sensitivity in a wide pressure range (0.002–7 kPa). This study introduces the carbon aerogel as an excellent choice for fabricating the 3D tactile sensor to capture various signals of human motions.The Supporting Information is available free of charge at <a class="ext-link" href="/doi/10.1021/acssuschemeng.1c02051?goto=supporting-info">https://pubs.acs.org/doi/10.1021/acssuschemeng.1c02051</a>.<a class="ref internalNav" href="#sec2">Experimental Section</a>; height of the CNF; FT-IR spectrum of the CNF; lamellar surfaces of CNF<sub>0.45%</sub>, CNF<sub>1.8%</sub>, CNF<sub>0.45%</sub>–C, and CNF<sub>1.8%</sub>–C; SEM images of aerogels before annealing; digital photographs of the as-prepared aerogels and carbon aerogels; XRD and Raman patterns of CNF<sub><i>X</i>%</sub>–C; microstructures of CNF aerogels (CNF<sub>0.9%</sub>) before and after annealing; digital photographs of the as-prepared aerogels and carbon aerogels before and after compression; compressibility of CNF<sub><i>X</i>%</sub>–C; SEM images of CNF<sub><i>X</i>%</sub>–C after 10,000 cycles at 50% strain; lamellar thicknesses of CNF<sub><i>X</i>%</sub>–C; <i>R</i>/<i>R</i><sub>0</sub> of CNF<sub>0.9%</sub>–C and its linear sensitivity; and comparison of pressure detection limit of CNF<sub>0.9%</sub>–C (<a class="ext-link" href="/doi/suppl/10.1021/acssuschemeng.1c02051/suppl_file/sc1c02051_si_001.pdf">PDF</a>)Compression at 90% strain for one cycle (<a class="ext-link" href="/doi/suppl/10.1021/acssuschemeng.1c02051/suppl_file/sc1c02051_si_002.mp4">MP4</a>)Finite element analysis of thin lamella (<a class="ext-link" href="/doi/suppl/10.1021/acssuschemeng.1c02051/suppl_file/sc1c02051_si_003.mp4">MP4</a>)Finite element analysis of thick lamella (<a class="ext-link" href="/doi/suppl/10.1021/acssuschemeng.1c02051/suppl_file/sc1c02051_si_004.mp4">MP4</a>)Finite element analysis of compression from the <i>x</i> direction (<a class="ext-link" href="/doi/suppl/10.1021/acssuschemeng.1c02051/suppl_file/sc1c02051_si_005.mp4">MP4</a>)Finite element analysis of compression from the <i>y</i> direction (<a class="ext-link" href="/doi/suppl/10.1021/acssuschemeng.1c02051/suppl_file/sc1c02051_si_006.mp4">MP4</a>)Finite element analysis of compression from the <i>z</i> direction (<a class="ext-link" href="/doi/suppl/10.1021/acssuschemeng.1c02051/suppl_file/sc1c02051_si_007.mp4">MP4</a>)This article has not yet been cited by other publications.
chemistry, multidisciplinary,engineering, chemical,green & sustainable science & technology
What problem does this paper attempt to address?