Evolution of Surface Structure on Pd–Cl/Alumina Catalyst During CO Purification Process

Luyang Qiao,Zhangfeng Zhou,Yunyun Zeng,Shanshan Zong,Dongjie Xu,Yuangen Yao
DOI: https://doi.org/10.1007/s10562-022-03981-w
IF: 2.936
2022-04-11
Catalysis Letters
Abstract:Eliminating hydrogen from CO via preferential oxidation is an important process in Coal to Ethylene Glycol technology for achieving target products with high yield. During the reaction, applied Pd–Cl/alumina catalyst inevitably experienced structural reconstruction stem from reaction conditions. The deactivation behavior of catalyst was clarified via spectroscopic and microscopic observations. It proposed that surface evolutions about metal sintering should be primarily responsible for the degradation of catalytic efficiency. Owing to chlorine effusion, dependent ferrous contamination and Pd aggregation was emerged on catalyst during the operation. The detachment of coordinative chlorine from active sites in the form of hydrogen chloride favored the accessing of adsorbate on Pd sites which further accelerated the coalescence of clusters. Despite the textural perturbation about porosity and surface area was negligible, on the other hand, the elimination of surface hydroxyls may contribute much for surface passivation and undermined Pd–Cl-Al interfacial interactions.Graphical AbstractDiagram illustrated the surface evolutions of catalyst during the operation in hydrogen preferential oxidation.
chemistry, physical
What problem does this paper attempt to address?