Pentlandite: Preparation, hydrogen reduction in the presence of lime to yield an iron-nickel alloy

I. D. Shah,P. L. Ruzzi
DOI: https://doi.org/10.1007/bf02653690
1978-09-01
Metallurgical Transactions B
Abstract:The present paper describes the hydrogen reduction of synthetic pentlandite and pentlandite concentrate in the presence and the absence of added calcium hydroxide. Synthetic pentlandite was prepared by heating a stoichiometric mixture of an iron-nickel alloy and sulfur for about 10 days at 473 to 723 K. Differential thermal analysis (DTA) apparatus was used to study the thermal decomposition of the synthetic pentlandite. Hydrogen reduction of synthetic pentlandite in the presence and the absence of added Ca(OH)2 was studied at 673 to 1023 K in a thermogravimetric apparatus. Additions of Ca(OH)2 to penlandite accelerated the reduction rates. An acetic acid leach of a product obtained by H2 reduction of a mixture of pentlandite and Ca(OH)2 yielded a leach residue containing mainly an iron-nickel alloy. The iron and nickel content in the leach residue averaged about 44 pct iron and 52 pct nickel with recoveries of about 82 pct iron and 94 pct nickel.
What problem does this paper attempt to address?