Microstructural evolution and mechanical behavior of Co‐free (Fe40Ni30Cr20Al10)100‐x Ti x high‐entropy alloys

Junchen Liu,Zhenfei Jiang,Weiping Chen,Haolun Fan,Zhiqiang Fu
DOI: https://doi.org/10.1002/adem.202300946
IF: 3.6
2023-09-23
Advanced Engineering Materials
Abstract:In this work, microstructural evolution and mechanical behavior of Co‐free (Fe40Ni30Cr20Al10)100‐x Ti x (x = 0, 2, 4, 6 and 8 at.%) high‐entropy alloys (HEAs) were investigated. All as‐cast HEAs consist of face‐centered cubic (FCC) and body‐centered cubic (BCC) structured phases, wherein the BCC‐structured phase is composed of disordered BCC (A2) and ordered BCC (B2) phases. The HEAs show FCC dendrite and BCC inter‐dendrite microstructure when x ≤ 4. As the Ti content increases to 6 and 8 at.%, the microstructure has evolved from dendrite structures to complex lamellar structures, leading to a significant loss in ductility. With the increase of Ti, the strength was enhanced with the sacrifice of ductility. The (Fe40Ni30Cr20Al10)96Ti4 alloy exhibits promising combinations of strength and ductility, displaying a yield strength of 680 MPa, an ultimate tensile strength of 1132 MPa, and a total elongation of 16.6%. The simple FCC+BCC dendrite microstructure and optimal content of the BCC‐structured region containing A2+B2 phases are responsible for the excellent tensile properties of the as‐cast (Fe40Ni30Cr20Al10)96Ti4 HEA. Our work suggests that good combinations of strength and ductility of low‐cost Co‐free FeNiCrAl‐based HEAs can be achieved by tailoring Ti addition. This article is protected by copyright. All rights reserved.
materials science, multidisciplinary
What problem does this paper attempt to address?