A novel adsorptive and photocatalytic system for dye degradation using ZIF-8 derived carbon (ZIF-C)-modified graphene oxide nanosheets

Mengjie Qiu,Wen Xu,Siman Chen,Zhaoping Jia,Yucheng Li,Jing He,Luying Wang,Jiandu Lei,Can Liu,Jing Liu
DOI: https://doi.org/10.1016/j.jtice.2023.104674
IF: 5.477
2023-01-22
Journal of the Taiwan Institute of Chemical Engineers
Abstract:Highlights • Cellulose-based carbon aerogel supported ZIF-8 derived carbon (ZIF-C) modified graphene oxide heterostructured composites (ZIF-GO/CCA) was successfully synthesized. • ZIF-GO/CCA has excellent adsorption and photocatalytic effect on organic dye in water. • CCA provided a large specific surface area and ZIF-C (with ZnO and g-C3N4) provided plenty of adsorption-photocatalytic active sites. • GO with lower Fermi level energy can served as an excellent electron accepter to reduce the band gap of ZIF-C and enhanced the separation ability of the e −/ h + pairs. • The removal efficiency of malachite green by ZIF-GO/CCA reached 96%, and the removal capacity reached 1152 mg· g − 1 after 120 min of reaction. Background Aerogels have attracted widespread interest in adsorption and photocatalysis. The effect of single aerogel material cannot meet the demand and we can enhance the adsorption and photocatalysis efficiency via adding other materials such as ZIF-8 and graphene oxide (GO). Methods We developed an adsorptive and photocatalytic system of ZIF-GO/CCA using a cellulose-based carbon aerogel (CCA) for the fabrication of GO nanosheets modified with ZIF-8-derived carbon (ZIF-C), followed by pyrolysis. The characteristics were evaluated using SEM, HRTEM, BET, XRD, XPS, UV–vis DRS, ESR, PL, EIS and LC-MS analysis. Significant findings CCA exhibit hierarchical porosity and conductive network, which provides abundant active sites for dye adsorption and degradation. ZnO and g-C 3 N 4 were formed after the incorporation of ZIF-C into GO to, promote charge separation. In the presence of 1ZIF-GO/CCA and at an initial concentration of 300 mg·L −1 MG, the removal of MG exceeded 96%. The removal capacity reached 1152 mg·g −1 after adsorption-photocatalysis for 120 min. 1ZIF-GO/CCA showed the largest specific surface area (375.059 m 2 ·g −1 ). GO served as an excellent electron accepter to enable fast electron transfer from the ZIF-C to the conduction band of GO. The narrower bandgap (2.06 eV) and lower resistance during charge transfer promoted the separation of e − / h + and contributed to the higher photocatalytic activity of ZIF-GO/CCA. Further, ZIF-GO/CCA showed increased recyclability. The plausible photocatalytic mechanism for the 1ZIF-GO/CCA was discussed. Graphical abstract Download : Download high-res image (179KB) Download : Download full-size image
engineering, chemical
What problem does this paper attempt to address?