Abstract:Bimetallic oxides have received considerable attention as anodes for lithium/sodium-ion batteries (LIBs/SIBs) due to their high electrochemical activity and theoretical specific capacity. However, their cycling performance is limited by large volume variation, severe aggregation, and pulverization of bimetallic oxide nanoparticles during repeated metal ion insertion/extraction processes. Herein, bimetallic antimony–vanadium oxide nanoparticles embedded in graphene (SbVO<sub>4</sub>/G) composites are prepared by a one-step hydrothermal method. Bimetallic SbVO<sub>4</sub> with abundant redox reaction sites can provide high specific capacity by a multi-electron reaction. A robust graphene substrate can not only alleviate volume expansion but also prevent aggregation and collapse of highly active bimetallic SbVO<sub>4</sub>. Due to the excellent synergy between the two building components, SbVO<sub>4</sub>/G hybrids exhibit excellent electrochemical activity, structural stability, and electrochemical performance. When employed as anodes for LIBs and SIBs, SbVO<sub>4</sub>/G composites display excellent cycling performance (1079.5 mAh g<sup>–1</sup> at 0.1 A g<sup>–1</sup> after 150 cycles for LIBs and 401.6 mAh g<sup>–1</sup> at 0.1 A g<sup>–1</sup> after 450 cycles for SIBs) and impressive rate capability. This work demonstrates that SbVO<sub>4</sub>/G composites are promising anodes for both LIBs and SIBs.The Supporting Information is available free of charge at <a class="ext-link" href="/doi/10.1021/acsami.0c21676?goto=supporting-info">https://pubs.acs.org/doi/10.1021/acsami.0c21676</a>.Pore size of pure SbVO<sub>4</sub> and SbVO<sub>4</sub>/G; GCD profiles of pure SbVO<sub>4</sub> at 0.1 A g<sup>–1</sup>; average discharge specific capacity of SbVO<sub>4</sub>/G and pure SbVO<sub>4</sub> as LIB anodes at different current densities; GCD curves of pure SbVO<sub>4</sub> and SbVO<sub>4</sub>/G composite electrodes at current densities of 0.1–3.0 A g<sup>–1</sup>; CV curves of pure SbVO<sub>4</sub> electrodes in SIBs at 0.2 mV s<sup>–1</sup>; GCD profiles of pure SbVO<sub>4</sub> electrodes in SIBs at 0.1 A g<sup>–1</sup>; Nyquist plots of SbVO<sub>4</sub>/G and pure SbVO<sub>4</sub> in SIBs; and SEM images of the fully discharged SbVO<sub>4</sub>/G electrode for LIBs and SIBs after 50 cycles (<a class="ext-link" href="/doi/suppl/10.1021/acsami.0c21676/suppl_file/am0c21676_si_001.pdf">PDF</a>)This article has not yet been cited by other publications.
materials science, multidisciplinary,nanoscience & nanotechnology
What problem does this paper attempt to address?