Role of vacancy type defects on microstructural and optoelectronic property of CdS wurtzite nanoparticles

Samiran Mandal,Dhanadeep Dutta,Sk Irsad Ali,Prosenjit Ghosh,Atis Chandra Mandal
DOI: https://doi.org/10.1016/j.molstruc.2024.137734
IF: 3.841
2024-05-01
Journal of Molecular Structure
Abstract:In this research work we have prepared CdS nanoparticles (NPs) without using any capping agent via chemical route. The five individual part of the sample was calcined with five different calcination temperatures, i.e. 450°C, 500°C, 550°C, 600°C and 650°C, respectively. The each individual calcined sample was characterized by different spectroscopic analysis such as X–ray diffraction (XRD), transmission electron microscopy (TEM), positron annihilation lifetime spectroscopy (PALS), optical absorption spectroscopy (OA) and fluorescence spectroscopy (FL). The particle sizes measured from XRD analysis were found to be 66–74 nm with wurtzite lattice structure. The trend of variation of size of the particles was correlated with the outcomes from TEM histograms as well as Williamson Hall (W–H) analysis. All the samples showed quantum confinement behaviour compared to bulk sample. The PALS study revealed the increase of the size of vacancy–like defects with calcination temperature, which impacted on an improvement of the intensity of visible fluorescence emission peaks around the wavelength 475 nm (blue), 520 nm (Green) and 670 nm (red). The intense luminescent characteristics of the sample can be utilized in various advancement of optoelectronic technology.
chemistry, physical
What problem does this paper attempt to address?