An Efficient Plasma Regeneration of As-Poisoned V2o5-Based Catalyst for Simultaneous Poison Removal and Activity Enhancement

Yong Yin,Kezhi Li,Si Jiang,Yue Peng,Tianle Zhu,Yifei Sun,Junhua Li,Xiang Li
DOI: https://doi.org/10.1016/j.cej.2024.156141
IF: 15.1
2024-01-01
Chemical Engineering Journal
Abstract:Regeneration of highly toxic Arsenic (As) poisoned SCR catalysts is a huge challenge, because the strong interactions between As and the active component often leads to the loss or damage of active sites during the regeneration process. Herein, we develop a low-temperature plasma regeneration method that not only selectively removes As but also preserves the active components for commercial V2O5-WO3/TiO2 catalyst. More intriguingly, the catalyst after plasma regeneration achieves a significant catalytic performance enhancement, far surpassing the fresh V2O5-WO3/TiO2 catalyst. Under optimized regeneration conditions, the regenerated catalyst exhibits an As removal rate exceeding 99.5 +/- 0.2 % within 240 s, and a reaction rate value that was 18.6 and 3.4 times of the poisoned and fresh catalyst. Structural characterization reveals that the enhanced intrinsic activity of regenerated catalyst mainly stems from the As complete removal and subsequent transformation of monomeric VOx species into polymeric ones under H(2 )plasma environment. Multiple spectroscopic monitoring techniques unveil three stages in the plasma treatment process: (1) As reduction and removal, (2) surface polymerization of VOx species, and (3) vanadium embedded into TiO2 lattice. At low temperatures, the well regenerated catalysts with abundant polymeric VOx facilitate the nitrate-assisted dehydrogenation of adsorbed NH3 to key NH2 intermediates, thereby achieving superior NH3-SCR catalytic performance. This study not only provides a rapid regeneration strategy for poison selective separation from spent catalysts but also offers new insights into the precise control and design of active sites.
What problem does this paper attempt to address?