DIRECT FORMATION OF LA(FE,SI)(13) PHASE BY DIRECTIONAL SOLIDIFICATION IN SLOW COOLING RATE

J. Liu,Jianwei Dong,Yang Shao
2014-01-01
Abstract:Direct formation of the La(Fe, Si)(13) phase has been realized by extremely slow cooling in directional solidification technique. A large amount of this magnetocaloric phase of about 85% was found in the as-solidified state. Correspondingly, magnetic entropy change of 13.5 J/kgK under an applied field of 2 T was obtained around 202 K for the alloy directionally solidified in a cooling rate of 0.005 K/s.