Comparison of the Thermal Stability of Lithiated Graphite in LiBOB EC/DEC and in LiPF[sub 6] EC/DEC

Jun Jiang,J. R. Dahn
DOI: https://doi.org/10.1149/1.1592911
2003-01-01
Electrochemical and Solid-State Letters
Abstract:Accelerating rate calorimetry (ARC) has been used to compare the thermal stability of lithiated mesocarbon microbeads (MCMB) in the presence of saturated lithium bis(oxalato)borate (LiBOB) in ethylene carbonate (EC)/diethyl carbonate (DEC) (about 0.8 M) and in EC/DEC (1.0 M). The exothermic reaction between lithiated MCMB and LiBOB EC/DEC electrolyte does not proceed strongly until about 170°C but it begins at about 80°C for lithiated MCMB in EC/DEC. We believe that LiBOB electrolytes offer significant advantages for cell abuse tolerance compared to electrolytes, at least as far as anode/electrolyte reactions are concerned. © 2003 The Electrochemical Society. All rights reserved.