Syntheses, Characterization, and in Vitro Degradation of Ethyl Cellulose-graft-poly(ε-caprolactone)-block-poly(l-lactide) Copolymers by Sequential Ring-Opening Polymerization

Weizhong Yuan,Jinying Yuan,Fengbo Zhang,Xu‐Ming Xie
DOI: https://doi.org/10.1021/bm0610018
2007-01-01
Biomacromolecules
Abstract:Well-defined ethyl cellulose-graft-poly(ε-caprolactone) (EC-g-PCL) graft copolymers were successfully synthesized via ring-opening polymerization (ROP) of ε-caprolactone (CL) with an ethyl cellulose (EC) initiator and a tin 2-ethylhexanoate (Sn(Oct)2) catalyst in xylene at 120 °C. Then, novel ethyl cellulose-graft-poly(ε-caprolactone)-block-poly(l-lactide) (EC-g-PCL-b-PLLA) graft-block copolymers were prepared by ROP of l-lactide (L-LA) with a hydroxyl-terminated EC-g-PCL macroinitiator and Sn(Oct)2 catalyst in bulk at 120 °C. Various graft and block lengths of EC-g-PCL and EC-g-PCL-b-PLLA copolymers were obtained by adjusting the molar ratios of CL monomer to EC and the L-LA monomer to CL. The thermal properties and crystalline morphologies of EC-g-PCL and EC-g-PCL-b-PLLA copolymers were different from those of linear PCL. The in vitro degradation rate of EC-g-PCL-b-PLLA was faster than those of linear PCL and EC-g-PCL due to the presence of PLLA blocks.
What problem does this paper attempt to address?