Hot Tearing Susceptibility of Mg-Zn-Y-Zr Alloys

En–Hou Han
2009-01-01
Abstract:Magnesium alloys are prone to hot tearing basically due to their long solidification range. Ternary Mg-Zn-Y (ZW series) alloys are the base of some new high strength wrought magnesium alloys and tend to hot tearing during DC casting. Some of ZW alloys including ZW22, ZW42, ZW44, ZW26 and ZW62 alloys are selected, aiming at understanding the relationship among hot tearing susceptibility and solidification pathways, residual liquid at the last stage of solidification and Zr refinement etc. by constrained rod casting (CRC) in a steel mold and cooling curve thermal analysis. Hot tearing susceptibility is found in the investigated alloys as follows: ZW62 without Zr additionZW62ZW22, and both ZW42 and ZW44ZW26. The highest hot tearing susceptibility of ZW62 alloy without Zr addition releates to the following reasons: the longest freezing range; after dendrite coherency, the formation of W-phase worsen the liquid flow and interdendritic feeding; less residual liquid and the solid fraction increasing slowly in the last stage of solidification; bulky and well-branched dendritic grains.
What problem does this paper attempt to address?