SnO2 As Advanced Anode of Alkali‐Ion Batteries: Inhibiting Sn Coarsening by Crafting Robust Physical Barriers, Void Boundaries, and Heterophase Interfaces for Superior Electrochemical Reaction Reversibility

Shiqiang Zhao,Christopher D. Sewell,Ruiping Liu,Songru Jia,Zewei Wang,Yanjie He,Kehong Yuan,Huile Jin,Shun Wang,Xueqin Liu,Zhiqun Lin
DOI: https://doi.org/10.1002/aenm.201902657
IF: 27.8
2019-01-01
Advanced Energy Materials
Abstract:Superior reaction reversibility of electrode materials is urgently pursued for improving the energy density and lifespan of batteries. Tin dioxide (SnO 2 ) is a promising anode material for alkali‐ion batteries, having a high theoretical lithium storage capacity of 1494 mAh g − based on the reactions of SnO 2 + 4Li + + 4e − ↔ Sn + 2Li 2 O and Sn + 4.4Li + + 4.4e − ↔ Li 4.4 Sn. The coarsening of Sn nanoparticles into large particles induced reaction reversibility degradation has been demonstrated as the essential failure mechanism of SnO 2 electrodes. Here, three key strategies for inhibiting Sn coarsening to enhance the reaction reversibility of SnO 2 are presented. First, encapsulating SnO 2 nanoparticles in physical barriers of carbonaceous materials, conductive polymers or inorganic materials can robustly prevent Sn coarsening among the wrapped SnO 2 nanoparticles. Second, constructing hierarchical, porous or hollow structured SnO 2 particles with stable void boundaries can hinder Sn coarsening between the void‐divided SnO 2 subunits. Third, fabricating SnO 2 ‐based heterogeneous composites consisting of metals, metal oxides or metal sulfides can introduce abundant heterophase interfaces in cycled electrodes that impede Sn coarsening among the isolated SnO 2 crystalline domains. Finally, a perspective on the future prospect of the structural/compositional designs of SnO 2 as anode of alkali‐ion batteries is highlighted.
What problem does this paper attempt to address?