Thermal Decomposition Kinetics, Reaction Mechanism, and Hazard Evaluation of the Hydroxylamine Sulfate Solution Doping Fe3+

Xiaoliang Zhang,Guangyuan Tao,Li Wang,Jiawei Fang,Yufei Xie,Tingting Deng,Jun Zhang
DOI: https://doi.org/10.1016/j.tca.2023.179535
IF: 3.5
2023-01-01
Thermochimica Acta
Abstract:To study the stability of hydroxylamine sulfate (HAS) when mixed with metal ions (especially Fe3+), the effect of Fe3+ doping on the thermal decomposition of HAS was studied by differential scanning calorimeter. The results indicate that HAS decomposes at 365-376 K and average thermal effect of P1 and P2 are approximately 632.6 J/g and 66.9 J/g, respectively. Fe3+ increases thermal effect of P1 and P2, but it decreases the initial decomposition temperature (To) of P1, and delays the To of P2. The density functional theory calculations results reveal a detailed 8-step reaction model of HAS decomposition with the formation of NH3OH+ as the key step. Notably, Fe3+ affects the thermal decomposition process of HAS by forming a coordination compound Fe(NH2OH)3+ 6 with NH2OH. In addition, model-free method prediction shows that Fe3+ reduces the kinetic parameters and the thermal hazard parameters.
What problem does this paper attempt to address?