Origin of Strong Metal-Support Interactions Between Pt and Anatase TiO2 Facets for Hydrodeoxygenation of M-Cresol on Pt/TiO2 Catalysts

Xiaoxia Wu,Chang-jun Liu,Hua Wang,Qingfeng Ge,Xinli Zhu
DOI: https://doi.org/10.1016/j.jcat.2023.01.023
IF: 7.3
2023-01-01
Journal of Catalysis
Abstract:Metal/reducible metal oxide catalysts are widely used in hydrodeoxygenation (HDO) reactions for upgrading bio-oil to produce chemicals and fuel components. Under such strong reducing condition, the strong metal-support interaction (SMSI) should take place, however, few work has been devoted to understand the effect of facet of metal oxide on the SMSI and its consequence on HDO performance. Herein, Pt supported on anatase TiO2 with varying dominative exposed facets of (101), (100) and (001) were prepared and tested in HDO of m-cresol at 350 degrees C and atmosphere H2 pressure. The degree of SMSI of Pt/TiO2 is strongly dependent on the facet of TiO2 when reduced at 350 degrees C, and the degree of encapsulation decreases following the order of Pt/TiO2-100 > Pt/TiO2-001 > Pt/TiO2-101. The encapsula-tion correlates well with the reduction degree of TiO2 and the location of oxygen vacancy, which are resulted from varied oxygen vacancy formation and anisotropic diffusion rates in different facets. The intermediate SMSI is achieved on TiO2-001, which creates the maximal density of Pt-Ov-Ti3+ sites at the interfacial perimeter of TiOx/Pt for deoxygenation of m-cresol, resulting in the highest reaction rate and turnover frequency (TOF) while the lowest activation energy (Ea). In contrast, the maximum SMSI on TiO2-100 leads to the lowest deoxygenation rate while the highest Ea. This work provides insight into facet dependent SMSI of Pt/TiO2 and indicates the HDO activity can be finely tailored by tuning the facet of TiO2.(c) 2023 Elsevier Inc. All rights reserved.
What problem does this paper attempt to address?