Regulating the Anode Corrosion by a Tryptophan Derivative for Alkaline Al-Air Batteries

Yue Huang,Lei Guo,Qiao Zhang,Wei Shi,Wei Feng,Faheem Abbas,Xingwen Zheng,Senlin Leng,Yujie Qiang,Viswanathan S. Saji
DOI: https://doi.org/10.1021/acs.langmuir.3c00032
IF: 3.9
2023-01-01
Langmuir
Abstract:Screening a green corrosion inhibitor that can prevent Al anode corrosion and enhance the battery performance is highly significant for developing next-generation Al-air batteries. This work explores the non-toxic, environmentally safe, and nitrogen-rich amino acid derivative, N(α)-Boc-l-tryptophan (BCTO), as a green corrosion inhibitor for Al anodes. Our results confirm that BCTO has an excellent corrosion inhibition effect for the Al-5052 alloy in 4 M NaOH solution. An optimum inhibitor addition (2 mM) has increased the Al-air battery performance; the corrosion inhibition efficiency was 68.2%, and the anode utilization efficiency reached 92.0%. The capacity and energy density values increased from 990.10 mA h g-1 and 1317.23 W h kg-1 of the uninhibited system to 2739.70 mA h g-1 and 3723.53 W h kg-1 for the 2 mM BCTO added system. The adsorption behavior of BCTO on the Al-5052 surface was further explored by theoretical calculations. This work paves the way for constructing durable Al-air batteries through an electrolyte regulation strategy.
What problem does this paper attempt to address?