Recycling Municipal Solid Waste Incineration Fly Ash in Super-Lightweight Aggregates by Sintering with Clay and Using SiC As Bloating Agent.

Siyu Han,Yingchun Song,Tongyao Ju,Yuan Meng,Fanzhi Meng,Mengzhu Song,Li Lin,Mengdan Liu,Jinglin Li,Jianguo Jiang
DOI: https://doi.org/10.1016/j.chemosphere.2022.135895
IF: 8.8
2022-01-01
Chemosphere
Abstract:Municipal solid waste incineration (MSWI) fly ash is classified as hazardous waste and requires proper treatments. Sintering of MSWI fly ash for the production of lightweight aggregate (LWA) is a promising treatment technology, while the dependence on natural bloating clay to produce high quality LWA has limited its wide application. In this study, by using SiC as a bloating agent, normal clay could be used to produce superlightweight aggregate (bulk density <500 kg/m(3)) with MSWI fly ash. Effects of SiC addition amount, sintering temperature and duration on LWA performance were studied. The results showed that LWA with SiC addition of 0.1-0.5 wt% had significant expansion at sintering temperature of 1120 degrees C-1160 degrees C. The optimal conditions were 0.3 wt% SiC addition and sintering at 1120 degrees C for 30 min, and the bulk density could reach 212 kg/m(3) with other properties meeting the LWA standard (GB/T 17431.1-2010). Further, the heavy metal leaching toxicity was significantly decreased after sintering and met the MSWI fly ash utilization standard (HJ 1134-2020). The X-ray diffraction results revealed the formation of a complex diopside-based phase after sintering. This study provides a new approach for recycling MSWI fly ash in LWA without dependence on specific clay resources, and makes this technology wider applicability.
What problem does this paper attempt to address?