Influence of Oxygen and Zirconium Contents on The Mechanical Properties of Ti-23Nb-0.7Ta-Zr-O Alloys

Kunlun Si,Xu Wang,Zhaolong Yin,Yi Yang,Songquan Wu,Geping Li,Kai Zhang,Hao Wang,Aijun Huang
DOI: https://doi.org/10.3390/met12061018
IF: 2.695
2022-01-01
Metals
Abstract:Ti-23Nb-0.7Ta-(0, 2)Zr-(1.2, 4, 6, 10)O alloys were prepared using a non-consumable arc-melting method. The tensile property of Ti-23Nb-0.7Ta-2Zr-1.2O alloys was tested at temperatures from -196 degrees C to 750 degrees C. The influence of O and Zr contents on thermal forgeability, room-temperature hardness and tensile property at 750 degrees C was investigated. For Ti-23Nb-0.7Ta-2Zr-1.2O alloy, the tensile strength decreased, and the ductility increased with the temperature increase. O and Zr had a negative effect on the thermal forgeability. Room-temperature hardness and tensile strength increased with an increase in O and Zr contents due to interstitial, solid solution strengthening and second-phase strengthening. All of the alloys exhibited high ductility at 750 degrees C with the total elongation above 34% and reductions in area above 80%.
What problem does this paper attempt to address?