A Comprehensive Analysis of Ultrasonic Pulse Current Reducing Hot Cracking in Inconel 718 Welds

Yajie Wang,Xiaoqiang Zhang,Daqing Wang,Jieshi Chen,Chun Yu,Junmei Chen,Jijin Xu,Ping Zhu,Hao Lu
DOI: https://doi.org/10.1016/j.matchar.2022.111840
IF: 4.537
2022-01-01
Materials Characterization
Abstract:A novel self-induced ultrasonic tungsten inert gas (U-TIG) welding has been successfully applied to weld the Inconel 718 sheet with thickness of 2 mm to reduce hot cracking. The welding arc, weld formation, microstructure and micro-hardness distribution between TIG and U-TIG welding were analyzed systematically. The relationship between micro-hardness and characteristics of grain size, grain orientation, grain boundary, segregation and recrystallization proportion in transition zone (from weld metal zone to heat affected zone) was investigated. The characteristics of sizes, disorientations and boundaries of adjacent grains, as well as the microstrain distributions in weld metal zones of TIG and U-TIG welds were analyzed contrastively. The results indicate that the welding arc with symmetrical shrinkage induced by ultrasonic pulse current greatly intensifies the central depression of the weld bead surface, which benefits the release of welding thermal stress. With the promoted transformation of coarse columnar dendrites to fine equiaxed dendrites with similar orientation in UTIG welds, the segregation in grain boundaries is greatly reduced, which reduces potential of the hot cracking initiation and propagation. In addition, the improvement of micro-hardness distribution is contributed by grain refinement and segregation dispersion in U-TIG welds.
What problem does this paper attempt to address?