Phase, domain, and microstructures in Sr 2+ substituted low‐temperature sintering PZT‐based relaxor ferroelectrics

Hao Chen,Jie Xing,Jingwen Xi,Tao Pu,Hong Liu,Jianguo Zhu
DOI: https://doi.org/10.1111/jace.17989
IF: 4.186
2021-07-09
Journal of the American Ceramic Society
Abstract:<p>The Ag-Pd internal electrode of multilayer piezoelectric ceramics need to be sintered below 1000 °C, and lead wires and components need to be welded with lead-free solder at 260 °C. PNN–PMW–PZT–<i>x</i>Sr piezoelectric ceramics with high Curie temperature (<i>T</i><sub>c</sub> &gt;260 °C) were synthesized at a low sintering temperature (960 °C) to meet the requirements of multilayer piezoelectric devices. The relationship between structures (phase, domain, and micro- structures) and electrical properties (piezo-/ferro- electric properties, and dielectric relaxation) in the Sr<sup>2+</sup> substituted ceramics were investigated. Rietveld refinement and Raman spectra show that Sr<sup>2+</sup> substitution can cause the phase change and increase the force constant of [BO<sub>6</sub>] octahedron. The piezoelectric response increases with increasing the content of the tetragonal phase (<i>CTP</i>) in the rhombohedral-tetragonal (R-T) coexisted ceramics. The ceramics with 0.6 mol% Sr<sup>2+</sup> substitution have minimum activation energy for domain wall movement (<i>E</i><sub>a</sub>) of 0.0362 eV which favors the formation of nanometer-sized domains, and possess excellent electrical properties (<i>d</i><sub>33</sub>=623 pC/N, <i>d</i><sub>33</sub><sup>*</sup>=783 pm/V, <i>T</i><sub>c</sub>=295 °C). The higher the <i>CTP</i>, the lower the <i>E</i><sub>a</sub>. The lower <i>E</i><sub>a</sub> favors the rotation of polarization direction and extension, and is beneficial to the generation of the nanometer-size domains, resulting in high piezoelectric properties.</p>
materials science, ceramics
What problem does this paper attempt to address?