Experimental Myringoplasty

L FEENSTRA,BWC VANDERVEN,FE KOHN,J FEIJEN
DOI: https://doi.org/10.1177/039139888000300612
1980-01-01
Abstract:Artificial eardrums made from biodegradable poly(D, L-lactic acid), poly(glycolic acid) and poly(ß-benzyl-L-aspartate-co-L-leucine) 50/50, and made from the microporous poly(tetrafluoroethylene) and bisphenol-A poly(carbonate) membranes were implanted into the ear and as a reference subcutaneously in rats. The implants were histologically examined for periods up to one year. From the biodegradable polymers studied the poly(ß-benzyl-L-aspartate-co-L-leucine) 50/50 evoked the least tissue reaction and the newly formed tympanic membranes are the best in terms of thickness and overall integrity. The microporous poly(tetrafluoroethylene) membrane can be considered as a valuable support for the formation of a reinforced tympanic membrane.