Origin of Water-Induced Deactivation of MnO<sub>2</sub>-Based Catalyst for Room-Temperature NO Oxidation: A First-Principles Microkinetic Study

Haiyang Yuan,Huagui Yang,P. Hu,Haifeng Wang
DOI: https://doi.org/10.1021/acscatal.1c01050
IF: 12.9
2021-01-01
ACS Catalysis
Abstract:MnO2-based catalysts exhibit remarkable activities in a room-temperature NO oxidation reaction (RT-NOR) but are challenged by water-induced deactivation. To improve the water-resistance driven by molecular-level mechanistic understanding, we herein report a systematic first-principles study and microkinetic simulation on elucidating the water-modulated RT-NOR mechanism on the notable beta-MnO2 catalyst. Results show that RT-NOR preferentially follows the Mars-van Krevelen mechanism on beta-MnO2(110) and that the coupling of lattice O (O-lat) with NO sitting on the surface Mn-cus site is the rate-limiting step. The presence of H2O results in a competitive effect against NO adsorbing on Mn-cus and inhibits NO2 formation. More crucially, the H2O-dissociated H species eventually accumulate on O-lat and are difficult to remove, which seriously poison the catalyst, although the Mn-cus-anchored OH intermediate can oxidize NO to NO2 via the nitrite/nitrate route. Weakening the H adsorption on O-lat, as well as the H2O adsorption on Mn-cus, is thus proposed as conductive to alleviating MnO2 deactivation. More essentially, we find that the vacancy formation energy of O-lat, E-f(O-vac), can serve as a unified descriptor for balancing H2O-resistance and catalytic activity; the excessively low E-f(O-vac) is the intrinsic origin of MnO2 susceptible to deactivation by H2O. By doping engineering guided by such a descriptor, we identify that the Cr-, Nb-, Ru-, or Rh-substituted doping can properly increase the E-f(O-vac) of MnO2 and weaken the H2O-induced deactivation in RT-NOR. These results may provide a theoretical basis on optimizing MnO2-based catalysts with improved H2O-resistance.
What problem does this paper attempt to address?