Effect Of Laccase Pretreatment On Hydrogen Peroxide Bleaching Of Bamboo Scmp

Li Bingyun,Zhan Huaiyu,Liang Chen,Fu Shiyu
2010-01-01
Abstract:The effect of laccase pretreatment on hydrogen peroxide bleaching of bamboo SCMP was discussed. The change of fiber surface after laccase pretreatment was analyzed by X-ray photoelectron spectroscopy (XPS). The results revealed that laccase pretreatment could improve the bleachability and brightness stability of SCMP. The optimal laccase pretreatment conditions were laccase 51U/g, HBT 0.5%, oxygen pressure 0.2MPa, pH 6 and temperature 50 degrees C. Under these conditions the brightness and PC number of pulp bleached by H(2)O(2) were 60%ISO and 2.03. The analysis of XPS showed that 91.19% of pulp fiber surface was covered with lignin after laccase treatment, but before the treatment only 55.58% of fiber surface was covered. Lignin precipitated on the fiber surface after laccase treatment could be easily removed in H(2)O(2) bleaching.