Strengthening Sintering Of Limonitic Nickel Laterite By Substituting Ferronickel Tailings For Sintering Fluxes
Deqing Zhu,Yuxiao Xue,Jian Pan,Congcong Yang,Zhengqi Guo,Hongyu Tian,Dingzheng Wang
DOI: https://doi.org/10.1007/978-3-030-36540-0_78
2020-01-01
Abstract:Ferronickel tailings, by-products from nickel laterite direct reduction-magnetic separation process, are now stored up in large quantities with low utilization because of the high MgO content. In this paper, ferronickel tailing with 5.82% Fe, 0.51% Ni, 44.08% SiO2, and 31.98% MgO was adopted to replace the traditional Mg-bearing flux, i.e. serpentine. The laboratory pot sintering tests show that, this new technique increases sinter productivity and tumble index by 4.12% and 10.63%, respectively, and reduces solid fuel rate by 6.35%. The mineralogical study of product sinter shows that the addition of ferronickel tailing contributes to the increase of the amount ofSFCAby 4.03%. Mg and Al elementswere found to migrate intomagnetite grains to form three types of spinel solid solutions, i.e. (Fe, Mg)Fe2O4, Fe (Fe, Al)(2)O-4, and (Fe, Mg)center dot(Fe, Al)(2)O-4. Meanwhile, eutectic compound melts were obtained by the co-melting of kirschsteinite (CaO center dot FeO center dot SiO2), monticellite (CaO center dot MgO center dot SiO2), and fayalite (2FeO center dot SiO2).