Performance deterioration and microstructure evolution of clay brick submitted to freeze-thaw cycles

Wenjuan Huan,Yunsheng Zhang,Guojian Liu,Peng Zhao
DOI: https://doi.org/10.3969/j.issn.1001-0505.2014.02.031
2014-01-01
Abstract:The changes of appearance,mass loss percentage and relative dynamic elastic modulus of clay brick submitted to freeze-thaw cycles were systematically studied.The mercury intrusion poro-simetry (MIP)was utilized to investigate the pore size distribution before and after freeze-thaw cy-cles.The X-ray computed tomography (CT)was also used to in situ quantitatively observe the evo-lution of the three-dimensional pore structure under freeze-thaw cycles.The results show that the frost damage is slight in the early stages.Macroscopic cracks appear on the surface after 35 freeze-thaw cycles and spalling occurs after 65 cycles.Mass is more sensitive when submitted to freeze-thaw cycles and shows a similar regulation as the relative dynamic elastic modulus with a first gradual increase,followed by a decrease.The pore structure analysis results show that the average pore size increases about 4 times after freeze-thaw cycles with coarse pores increasing by 23% in volume. Simultaneously,the number and the volume of pores with the volume of 0.01 to 0.1 mm3 increase evidently.The frost resistance of clay red brick is reduced consequently.
What problem does this paper attempt to address?