Mechanism of Weld with Trailing Impact Rolling to Control Residual Stresses Deformation and Hot Cracking
FAN Chenglei,Fang Hongyuan,TAO Jun,LI Ming
DOI: https://doi.org/10.3321/j.issn:1000-0054.2005.02.005
2005-01-01
Abstract:The plastic flow and the variation of the strain field in welds caused by impact rollers were analyzed numerically to study the effect of weld with trailing impact rolling (WTIR). The front impact roller causes transverse plastic compression strain in the weld which is in the brittle temperature range, which counteracts the tensile strain which leads to hot cracking. The rear impact roller stretches the weld longitudinally with transverse compressive plastic deformation of the weld, thus reducing the residual deformation and stresses in the bead. The experimental results show that the weld surface with WTIR is flat and smooth with no hot cracking in the weld. The longitudinal deflection deformation with WTIR is reduced by 90% while the transversal contraction deformation is reduced by 80% relative to an ordinary weld. The residual stresses in the weld are also greatly reduced.
What problem does this paper attempt to address?