Preparation and characteristics of a novel biodegradable antibiotics-eluting nanofiber-loaded bone scaffold

Jianting Gao,Guofeng Huang,Guojun Liu,Lei Ren,Changqing Chen,Zhenqi Ding
DOI: https://doi.org/10.3760/cma.j.issn.1001-9030.2016.11.005
2016-01-01
Abstract:Objective This study describes the preparation and characteristics of a novel biodegradable vancomycin-eluting nanofiber-loaded bovine deproteinized bone scaffold.Methods The solution of poly (D,L)-lactide-co-glycolide (PLGA) and vancomycin in 1,1,1,3,3,3-hexafluoro-2-propanol was prepared and then electrospun into nanofibers onto the surface of bovine deproteinized bone scaffold.The surface characteristic of the novel scaffold was scanned by scanning electron microscope.The in vitro release rate of vancomycin from the nanofiber-enveloped scaffolds was detected by an elution method.The in vitro antibacterial activity and cytocompatibility was also investigated.Results Vancomycin-eluting nanofiber membrane has a diameter of about 100-1 200 nm and a pore size of about 1-5 μm,closely attached on the surface of deproteinized bone scaffold.Vancomycin-eluting scaffolds released a sustained high concentrations of vancomycin in vitro (well above the minimum inhibitory concentration) for more than 4 weeks.The bacterial inhibition zone lasts for about 4 weeks.When the scaffold materials were co-cultured with rabbit mesenchymal stem cells,relative cell survival factor declined slowly to the minimum of about 93.8% on the 6th day,and then increased slowly,which had no significant difference statistically among three groups.Conclusion The new vancomycin-eluting nanofiber-loaded deproteinized bone scaffold can achieve sustained release of antibiotics,good cytocompatibility,and thus may be an ideal repair material for the prevention and treatment of infected bone defect.
What problem does this paper attempt to address?