Biocompatibility of Electrospun Poly (L-Lactic Acid)/poly (Ε-Caprolactone) Blending Nanofiber in Vitro

BAI Yi,CHEN Liang,PENG E-jun,WU Bo-lin,WANG Yu-xi,ZENG Xiao-yong,YE Zhang-qun
DOI: https://doi.org/10.3760/cma.j.issn.1001-9030.2012.11.048
2012-01-01
Abstract:Objective To explore the biocompatibility of electrospun poly (L-lactic acid)/poly (ε-caprolactone) (PLA/PCL) blending nanofibrous scaffolds in different composite ratios using adipose-derived stem cells (ADSCs).Methods PLA and PCL were blended in the weight composite ratios of 3∶ 1,2∶1 and 1∶ 1.They were synthesized to be nanofibrous scaffolds (NFS) by electrospinning technique.ADSCs isolated from the subcutaneous adipose tissue of a rabbit were seeded on the NFS,and the morphology of varied NFS at 1st,3rd and 7th day after inoculation was observed.Methyl thiazol tetrazolium (MTT) assay was used to investigate the proliferation of ADSCs on NFS in consecutive 7 days and attachment at 6 and 24 h.The living and dead cell staining was used to compare the number of living and dead ADSCs on NFS at 7th day.Results The diameters of three NFS were respectively (973 ±65),(617 ±44) and (432 ±24) nm.ADSCs on 1 ∶ 1 NFS demonstrated a larger quantity than the other two.Also,ADSCs proliferated faster on 1∶ 1 NFS than 3∶1 NFS and 2∶1 NFS at 6th,and 7th day (all P <0.05).The number of attached ADSCs on 1∶1 NFS whenever at 6 or 24 h was more than that on 3∶ 1 and 2∶1 NFS (all P < 0.05).The percentage of living ADSCs on the three NFS was (65.60 ±7.80)%,(69.16 ±8.30)% and (82.20 ± 10.20)% respectively.Conclusion The electrospun NFS of 1∶1 PLA/PCL blend showed excellent biocompatibility.
What problem does this paper attempt to address?