Effect Of Prior Deformation On Welding Microstructure Of Steel 304l

Wu Luo-Fei,Cheng Qiang,Li Zhu-Guo
DOI: https://doi.org/10.11868/j.issn.1001-4381.2015.000051
2017-01-01
Journal of Materials Engineering
Abstract:This subject was raised by an automotive company. Based on the welding design on the curved surface, the effect of prior deformation on the weld structure was studied. Metal active-gas welding was used on the T-joint and pre-deformed plates of austenitic stainless steel 304L to find the proper welding parameters and observe the effect of prior deformation on the microstructure. The proper parameters acquired are: the speed of the torch is 4mm/s, the speed of delivery of welding wire is 2. 5m/min and the voltage is 17V. In the T-joint and pre-deformed joint, the weld toes are in the zone with strain of 0 % and 30%. In the pre-deformed welding specimen, it was observed that the fusion zone and partially melted zone are narrowed, carbide precipitation and ferrites are found less. In all, the microstructure in the pre-deformed weld joints on 304L is more uniform.
What problem does this paper attempt to address?