Recycling of Copper Nickel from the Leaching Agent of Sodium Jarosite Slag by Extraction Method

Fang-bing FENG,Yun-guang WANG,Jing-yong XU,Hong LIU
DOI: https://doi.org/10.3969/j.issn.1006-0308.2017.03.007
2017-01-01
Abstract:sodium jarosite is resolved by stronger ammonia water, the copper and nickel should be extracted by LIX984 extraction agent and Bis phosphate (P204) separately after the leaching agent treated by hydrochloric acid.It is discussed that the effect of the extraction conditions, such as pH value in feed solution, the volume fraction, phase ratio (O/A), copper, nickel ionic concentration, extraction agent reextraction phase ratio (O/A) in organic phase on copper, nickel extraction rate.The results show: the volume fraction of LIX984 extraction agent is 20%, the pH value is 2.5, the phase ratio (O/A) is 1∶1, the average concentration of Cu2+ and Ni2+ is around 5g.The extraction rate of L-1, Cu2+ is about 92%, the re-extraction phase ratio (O/A) is 1∶1, the re-extraction rate of copper reach to 99%, when adjust the pH value in the extraction raffinate to 5.5, the extraction rate of nickel by P204 is over 98%, the re-extraction rate of nickel is about 91%.The extraction effect of copper and nickel by LIX984 and P204 extraction agent is significantly, which can extract copper and nickel in the sodium jarosite leaching agent selectively.
What problem does this paper attempt to address?