Behavior of accompanying rare earth during process of decomposing scheelite by sulfuric-phosphoric mixed acid

GUO Fu-liang,CHEN Xing-yu,ZHAO Zhong-wei,HE Li-hua,YANG Kai-hua,YANG Zhen
DOI: https://doi.org/10.19476/j.ysxb.1004.0609.2018.02.21
2018-01-01
The Chinese Journal of Nonferrous Metals
Abstract:The thermodynamic equilibrium diagrams for the distribution of species of accompanying rare earth(REE) at different pH values, sulfuric and phosphorous acid concentrations were drawn at 25 ℃. Using these diagrams, the technical methods for extracting rare earth and tungsten were found theoretically and tested by experiments. It appears that rare earth ions can be coordinated by phosphorous acid, sulfate anion or hereopolytungstate anion at different pH values. When the pH value is less than 1, rare earth ions coordinate with phosphorous acid or sulfate anion preferentially and transform to cation cluster. At the pH range of 1-3, rare earth ions coordinate with hereopolytungstate anion and transform to lanthanide containing anion cluster. These complexations are favorable to decompose rare earth minerals. The heteropoly acid can promote the decomposition of rare earth. When the mass fraction of WO3and rare earths in scheelite are 26.11% and 0.13%, and the concentration of sulfuric and phosphoric acid are 2.5 and 1 mol/L, respectively, the leaching rates of La, Ce, Nd reach 85.61%,45.68% and 47.03% at 90 ℃ for 5 h. Besides, rare earth and tungsten also can be extracted separately or simultaneously as the species of complexations difference.
What problem does this paper attempt to address?