Effect of annealing process on microstructure and properties of extruded TA15 alloy tube with large size

Shengchuan Chen,Xiuyong Li,Ruibo Chen,Baohui Zhu,Guoshuai Cai,Jun Liu,Shouquan Tang
DOI: https://doi.org/10.13251/j.issn.0254-6051.2017.05.037
2017-01-01
Abstract:Based on the existing production conditions,some extruded TA15 alloy tubes with large size were annealed at 700-850 ℃ in electric resistance furnace.Effect of annealing process on microstructure and properties of the extruded TA15 alloy tube was investigated.The results show that the faster the cooling rate and the higher the annealing temperature,the lower the yield strength and the yield ratio.Lower yield strength and preferable plasticity of the tube can be obtained when annealed at 850 ℃ and then water cooled,which is favorable to the subsequent rolling process with larger strain extent.