Effects of Oscillating Arc on Sidewall Penetration of Aluminum Alloy Thick Plate Welding

Laijun WU,Yibo LIU,Yafeng WANG,Qingjie SUN
DOI: https://doi.org/10.14158/j.cnki.1001-3814.2017.13.018
2017-01-01
Abstract:Lack of fusion on sidewall is a common welding defect in narrow gap welding of aluminum alloy thick plate. The lack of fusion on sidewall was solved through motor driven bending tip swinging to control oscillating arc's deflection. The effects of welding parameters on sidewall penetration of 6061-T6 aluminum alloy plate were studied by orthogonal experiments and single factor tests. The results show that the oscillating angle is the main factor that affects the sidewall penetration and follwed by the welding speed and dwell time at side wall. For U groove with bottom width of 10 mm and top width of 13 mm, the optimal welding parameters are oscillating angle of 50°, dwell time at side wall of 0.5 s, wire feeding speed of 11 m/min, and welding speed of 200 mm/min. Taking the optimal paramenters as reference, the single pass multilayer narrow gap welding of 40 mm thick 6061-T6 aluminum alloy plate was realised, and the joint has good sidewall fusion and the tensile strength of welded joint after heat treatment reaches 246.7 MPa.
What problem does this paper attempt to address?