Laser Welding Parameters and Tensile Properties of Partial Penetration Lap Joint for Stainless Train Body

WEN Peng,WU Ruifeng,WANG Xiuyi,AN Ji,WANG Xiaolong,ZHANG Yan
DOI: https://doi.org/10.3969/j.issn.1004-132X.2017.11.016
2017-01-01
Abstract:Partial penetration lap laser welding was used for 301L-H stainless steel train bodies to solve the heats and the weld distortion problems.The effects of focused laser spot diameter and weld-ing parameters were investigated with using fiber laser.Relationship among processing parameters and welding quality index like formation quality,heat trace on the surface,penetration shape and shear tensile performance,were concluded.The principles and methods were discussed for the selection of optimized parameters.For the combination of 0.8 mm and 1.5 mm high tensile strength plates,which were typically used for light weight train bodies,the outputs of laser machine should be over 2 kW, and the focused spot diameters should be over 0.4 mm if a large processing window was obtained to satisfy both appearance and mechanical requirements.For fiber laser with 0.4 mm spot diameter,the penetration should be less than 1 .4 mm to make the outside surfaces no heat traces,and the fusion width in the interfaces between inner and external plate should be more than 0.8 mm to make the ten-sile strength higher than that of resistance spot welding.For 301L-H stainless steel with tensile strength over 930MPa,the fractures are always located in the fusion zones at the interfaces between inner and external plates,so the tensile capacity is linearly related to the fusion widths in the interfaces.
What problem does this paper attempt to address?