Quantification of ZnO in nano ZnO/LDPE food packaging films and food simulant

Ying-chun SHI,Chang-ying HU,Jin-yu HUANG
DOI: https://doi.org/10.13995/j.cnki.11-1802/ts.201703040
2017-01-01
Abstract:Zinc oxide (ZnO) was determined in nano-zinc oxide food packaging and food simulants by microwave digestion with inductively coupled plasma atomic emission spectrometry (ICP-AES) and inductively coupled plasma mass spectrometry (ICP-MS).According to the European Union regulation (EU 10/2011),3% acetic acid was chosen and ultrapure water was used as food simulants,the test was carried out at 40 ℃ for 10 days.The amount of ZnO in food simulant was analyzed by ICP-AES and ICP-MS.The results showed the calibration curve of Zn was linear in the range of 0.1-5 mg/L with correlation coefficients no less than 0.9998.The spiked recoveries at three spiked levels were in the range of 91.2%-110.2% with relative standard deviations (RSD) of 0.3%-6.8%.The limit of detection (LOD) was 0.015 mg/L,0.03 mg/L and 0.03 μg/L respectively;the limit of quantitation (LOQ) was 0.05 mg/L,0.1 mg/L and 0.1 μg/L respectively.This method was precise,highly sensitive and accurate.This method was applied in determination of nano ZnO amount in three types of film and result was (4.71 ±0.19) g/kg,(9.20-±0.49) g/kg and 12.87 ±0.33 g/kg respectively.The amount of nano ZnO in 3% acetic acid food simulates at 40 ℃ for 10 days was (2.35 ±0.02) mg/kg,(3.54 ±0.01) mg/kg and (4.12 ±0.35) mg/kg respectively;the amount of nano ZnO in ultrapure water simulate at 40 ℃ for 10 days was (24.65 ±0.68) μg/kg,2(4.80 ± 1.25)μg/kg and (45.85 ±0.32) μg/kg,respectively.
What problem does this paper attempt to address?