Effect of NH4+ on the formation of secondary iron minerals and the removal of heavy metals

SONG Yong-wei,WANG He-ru,CAO Yan-xiao,ZHU Yi-han,ZHOU Li-xiang
DOI: https://doi.org/10.3969/j.issn.1000-6923.2018.06.014
2018-01-01
Abstract:In this study, the influence of initial pH, Fe2+ concentration, molar ratio of Fe/NH4+ on the Fe2+ bio-oxidation rate, total Fe deposition efficiency, and phases of secondary iron minerals in simulated AMD containingA. ferrooxidans was investigated. The Cr(VI) and As(III) removal efficiency of different iron minerals were compared. The results indicated that under the concentration of NH4+ was lower than that forA. ferrooxidanstolerance value, Fe2+ oxidation and total Fe removal through precipitation were not affected, 160, 80, and 20mmol/L of Fe2+could be completely oxidized by A. ferrooxidans within 72, 48, and 24h, and the average total Fe removal efficiency was 24.03%, 19.46%, and 8.13% at the end of the experiment (96h), respectively. In addition, in initial 160mmol/L Fe2+ system, when the molar ratio of Fe/NH4+=2.0 and pH=2.6, the secondary iron mineral obtained was pure schwertmannite; when the molar ratio of Fe/NH4+≤1.0 and pH≤2.3, ammonium jarosite began to occur in this system. Additionally, the Cr(VI) and As(III) removal efficiency of secondary iron minerals harvested from the Fe/NH4+=2.0systems differed (pH=2.6>pH=2.3>pH=2.0). The data obtained from this study demostrated that the removal efficiency of toxic elements was mainly influenced by the apparent structure and specific surface area of secondary iron minerals.
What problem does this paper attempt to address?