CoO Nanotubes Loaded on Graphene and Modified with Porphyrin Moieties for Colorimetric Sensing of Dopamine
Xin Zhao,Shuang Zhao,Shu Li,Xiuxiu Yao,Xixi Zhu,Wei Chen,Gaochao Fan,Zhenxue Liu,Qingyun Liu,Kang Yue
DOI: https://doi.org/10.1021/acsanm.1c01205
IF: 6.14
2021-08-25
ACS Applied Nano Materials
Abstract:In this paper, CoO nanotubes loaded on the surface of graphene oxide (GO) have been first modified by 5,10,15,20-tetrakis(4-carboxyl phenyl)porphyrin (Por) by a hydrothermal method. Por/CoO/GO exhibits excellent peroxidase-like activity, which is evaluated by virtue of the chromogenic substrate 3,3,5,5-tetramethylbenzidine (TMB). In the presence of H2O2, Por/CoO/GO nanoperoxidase can rapidly catalyze colorless TMB to be oxidized into blue oxTMB, which is distinguished visually in 1 min. The experimental data including fluorescence and electrochemistry data and radical scavengers confirm that the catalytic mechanism of Por/CoO/GO is ascribed to electron transfer between substrates, as well as produced active species (h+ and •O2–). Based on Por/CoO/GO nanoperoxidase, a fast colorimetric sensor for H2O2 has been established for a wide range of concentrations (0.1–3 mM) with a lower limit of detection (LOD = 0.2942 mM). Notably, the blue color of oxTMB can be gradually faded in the presence of dopamine (DA) with various concentrations. Thus, a fast, cheap, and convenient colorimetric sensor has been designed to monitor DA in a wide range (0.2–10 μM) with a much lower LOD (0.1391 μM). The Por/CoO/GO-based colorimetric platform has been validated by determining DA in real serum samples.The Supporting Information is available free of charge at https://pubs.acs.org/doi/10.1021/acsanm.1c01205.Preparation process of CoO/GO and Por/CoO/GO; kinetic test; assays of the peroxidase-like activity of Por/CoO/GO; assays of colorimetric H2O2 and DA; components of different systems (Table S1); comparison of kinetic parameters of different artificial nanoperoxidases (Table S2); linear range and LOD of different nanoenzyme-based colorimetric sensors for detection of DA (Table S3); molecular structure of 5,10,15,20-tetrakis(4-carboxyl phenyl)porphyrin (Por) (Figure S1); optimal conditions for the peroxidase-like activity of Por/CoO/GO (Figure S2); absorbance in the range of 500–800 nm for Por/CoO/GO5, Por/CoO/GO, and Por/CoO/GO15 (Figure S3); XRD pattern of pure CoO (Figure S4); and high-resolution XPS spectrum of N 1s of pure Por (Figure S5) (PDF)This article has not yet been cited by other publications.
materials science, multidisciplinary,nanoscience & nanotechnology