Abstract:Larger thermal stress can lead to capacity fade and safety issue of lithium-ion batteries. Thermal expansion is induced by thermal stress due to the temperature deviation during charge-discharge cycles. In this study, the thermal expansion behavior for a 38 Ah prismatic ternary battery is identified by presenting a three dimensional thermal-mechanical model. Corresponding experiments are conducted to measure the internal resistance and Young’s modulus that are decisive for the results. Then the model is validated by the temperature response at different discharge currents, and parameters sensitivity analysis is carried out to evaluate the uncertainty of the model. Based on the model, the temperature distribution is revealed over the cell that the temperature follows the sequence from high to low that is cell, positive tab, and negative tab; the temperature difference between two tabs is larger than that between positive tab and battery cell. The stress exhibits correlation with temperature gradient that enhanced von-Mises stress is observed at inner center of cell as elevated temperature levels. The simulation results also provide insight into the von-Mises stress and displacement along three directions (width, thickness and height) of the battery at different depth of discharge and current. It is found that larger thermal stress and expansion are observed with increasing current and depth of discharge, as well as at the boundary constraints. Besides, the battery expands more along the thickness direction and the tab portion where the temperature is higher. The maximum thermal average volume stain aroused by temperature difference during discharge at 1 C is 1.04×10−4.
What problem does this paper attempt to address?