Nonequilibrium Anionic Ring-Opening Polymerization of Tetraphenyltetramethylcyclotetrasiloxane (D-4(Me,ph)) Initiated by Sodium Isopropoxide

Xiyin Gao,Qian Wang,Hongjie Sun,Yongxia Tan,Zhijie Zhang,Zemin Xie
DOI: https://doi.org/10.1080/10426507.2013.860534
2014-01-01
Phosphorus Sulfur and Silicon and the Related Elements
Abstract:The nonequilibrium anionic ring-opening polymerization (NAROP) of tetraphenyltetramethylcyclotetrasiloxane (D-4(Me,Ph)) in the presence of initiator (sodium isopropoxide) and promoters including 12-crown-4, N-methyl-2-pyrrolidinone (NMP), N,N-dimethylformamide (DMF), and diglyme was investigated. It was found that the polymerization could be accelerated sharply by the increase of reaction temperature, as well as the mole ratio of promoter to initiator ([p]/ ratio). The NAROP rate of D-4(Me,Ph) decreased in the order of promoters: 12-crown-4>> NMP >DMF >diglyme. In the presence of NMP and sodium isopropoxide ([p]/ ratio = 3.0, 10h at 70 degrees C), the polydispersity index (PDI) of the poly(methylphenylsiloxane) obtained is 1.52, and the conversion rate of the monomer can reach over 90%. The byproduct pentaphenylpentamethylcyclopentasiloxane (D-5(Me,Ph)), which encountered in the 12-crown-4 promoted system upon prolonged reaction time, was not observed according to the Si-29 NMR of the reaction mixtures. In conclusion, NMP turned out to be the best choice among those promoters to realize the NAROP of D-4(Me,Ph).
What problem does this paper attempt to address?