Mechanism of Crack Initiation of Dissimilar Joints between 2219 Aluminum Alloy and 5A06 Aluminum Alloy

Chen Chao,Li Qingqing,Lin Sanbao,Zhou Jing,Fan Chenglei,Yang Chunli
2019-01-01
Rare Metal Materials and Engineering
Abstract:The crack initiation mechanism of dissimilar aluminum alloy welded joints was studied. The base metals were 2219 aluminum alloy and 5A06 aluminum alloy, while the filler wires were 2325 and 5B06. The microstructure was analyzed by optical microscope (OM), scanning electron micrograph (SEM) and energy dispersive spectroscopy (EDS). The results show that the weld hardness (HV) obtained by the 2325 is about 1000 MPa and that by 5B06 is about 800 MPa. Compared with that of the weld obtained by 2219 and 2325, the grain growth of HAZ (heat affected zone) of the weld obtained by 5A06 and 2325 is so weak that the joint softening phenomenon doesn't exist. The diffusion and segregation of Mg element and Cu element can be obviously observed in the welded fusion zone (FZ) obtained by 2325 and 5A06, and that by 5B06 and 2219. Compared with the welded joint obtained by 5B06 filler wire, the great cracking tendency can be found in dissimilar welded joint obtained by 2325 filler wire, because there is no obvious low melting eutectics in welded joint by 5B06 filler wire. Many low melting eutectics (Al2CuMg and CuAl2) are present in the welded joint by 2325 filler wire, and the Al2CuMg eutectics are fundamental cause for the crack initiation.
What problem does this paper attempt to address?