Extraction of rare earth and cobalt from leach residue of Nd-Fe-B waste by reductive leaching with iron powder
Haojie Du,Dong Wang,Liping Zhang,Wentao Li,Zhi Wang,Wanhai Xiao,Chunlin Ye,Haojie Du,Dong Wang,Liping Zhang,Wentao Li,Zhi Wang,Wanhai Xiao,Chunlin Ye
DOI: https://doi.org/10.1016/j.hydromet.2022.105942
IF: 4.217
2022-08-01
Hydrometallurgy
Abstract:After recovering rare earth from neodymium–iron–boron (Nd–Fe–B) magnet waste via oxidation roasting–hydrochloric acid leaching, extracting rare earths and cobalt from remaining leach residue, containing about 0.67% (w/w) RE and 0.36% Co, is environmentally and economically important. However, extracting valuable elements from low–grade minerals remains challenging. The purpose of this study is to accelerate the dissolution of rare earths and cobalt from leach residue of Nd–Fe–B waste (MWLR) under low acidity by adding iron as a reductant, which is conducive to destroying the main phase iron oxide. To optimize the leaching process of MWLR in a sulfuric acid system, the effects of reaction temperature, reaction time, sulfuric acid dosage, solid/liquid (S/L) ratio, reductant addition time and reductant dosage were investigated. Circa 87.9% Fe, 99.7% Co, 99.4% Nd, 73.2% Pr and 87.9% Ce were leached. Furthermore, kinetic results indicated that the leaching process, controlled by a combination of internal diffusion and surface chemical reaction, changed to a surface chemical reaction control in the presence of Fe added as the reductant. This research proposed and verified a way to extract low–grade rare earths and cobalt from MWLR, and investigated the mechanism of reductive leaching process.
metallurgy & metallurgical engineering