Preparation and biocompatibility of an electroactive polyaniline/poly(lactic-acid) scaffold

Ling-ling Wang,Zhi-ming Cui,Guan-hua Xu,Wei-dong Li,Guo-feng Bao,Yu-yu Sun,Jia-jia Chen,Jin-long Zhang
DOI: https://doi.org/10.3969/j.issn.2095-4344.0755
2018-01-01
Abstract:BACKGROUND: Previous studies have confirmed that polyaniline/poly(lactic‐acid) scaffold could promote the growth of neural stem cell processes in the condition of electrical stimulation. OBJECTIVE: To prepare an electroactive polyaniline/poly(lactic‐acid) scaffold and to investigate its biocompatibility with rat olfactory ensheathing cells. METHODS: Olfactory ensheathing cells of Sprague‐Dawley neonatal rats were inoculated onto the polyaniline/poly(lactic acid) film (experimental group) and poly lysine coating slides (control group). Cell proliferation and cell adhesion rate were detected, and the cells were observed with immunofluorescence histochemistry. RESULTS AND CONCLUSION: (1) Smooth and even polyaniline/poly(lactic acid) film was visible under electron microscopy, with a grid structure formed by fine fibers, and its conductivity was 1.5×10‐5 S/cm. (2) At 1, 3, 5, 7 days after co‐culture, the cell relative growth rates were all above 90%, and the cytotoxicity was graded I. (3) At 7 days after co‐culture, the cell adhesion rate in the experimental group was significantly higher than that in the control group (P < 0.05). (4) At 7 days after co‐culture, immunofluorescence results showed that there was no obvious difference between the two groups in the number or area of S‐100 positive cells (P > 0.05), while the cell perimeter in the experimental group was significantly higher than that in the control group (P < 0.05). To conclude, the prepared polyaniline/poly(lactic acid) film has good biocompatibility with olfactory ensheathing cells.
What problem does this paper attempt to address?