Hydroforming of an Automotive Torsion Beam with 780 MPa Advanced High Strength Steel

HAN Cong,HE Jiu-qiang,YUAN Shi-jian
DOI: https://doi.org/10.3969/j.issn.1674-6457.2016.05.008
2016-01-01
Abstract:ABSTRACT:Torsion beam is popular to be designed into a hollow closed section of high strength steel structure to satisfy the requirements of the load, installation space and the lightweight. However, there are springback, forming accuracy and other shortcomings during the forming of the advanced high strength steel. In this paper, a 780 MPa advanced high strength steel tor-sion beam was investigated using numerical simulation and experimental method. The effect of preform shape on hydroforming was mainly focused and the preform shape was optimized using a response surface model and the optimal preform shape was obtained. On the basis of this, the effect of loading path on hydroforming process of torsion beam was studied. The results show that the optimal preform shape of the torsion beam can be obtained when the press displacement is 62.2 mm and the guidance angle of lower die is 29.2 degrees. During hydroforming process, if the support pressure is too small or axial feeding is too large, wrinkling defect will occur. While the support pressure is too large or axial feeding is too small, feeding mainly concentrated in the end and less affected on expansion regions. When the axial feeding is 8%, it can effectively improve the wall thickness dis- tribution and avoid wrinkling defects. It can be known that the appropriate preform shape can effectively avoid flashing defects when hydroforming of a high strength steel torsion beam. At the same time, the control of loading paths is an effective way to avoid wrinkling and severe thinning and improve forming limit and forming precision.
What problem does this paper attempt to address?